eFunda: Properties of Carbon Steel ASTM A109 Temper 5
engineering fundamentals Carbon Steel ASTM A109 Temper 5
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
ASTM A109 Temper 5
Category Steel
Class Carbon steel

Composition
ElementWeight %
C  0.15 
Mn  0.60 
P  0.035 
S  0.04 
Si  0.30 (max) 
Mo  0.2 (min) 
Cu  0.20 (min) 
Nb  0.03 (min) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  