eFunda: Properties of Carbon Steel aisi 1213
engineering fundamentals Carbon Steel aisi 1213
Directory | Career | News | Standards | Industrial | SpecSearch®
Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI 1213
Category Steel
Class Carbon steel
Type Standard resulfurized and rephosphorized
Designations  Germany: DIN 1.0715
Italy: UNI 9 SMn23
Japan: JIS SUM 22
United Kingdom: B.S. 220 M07
United States: ASTM A108 , ASTM A29 , FED QQ-S-637 (1913) , SAE J403 , UNS G12130

Composition

ElementWeight %
C  0.13 (max) 
Mn  0.70-1.00 
P  0.07-0.12 
S  0.24-0.33 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 540  25  cold drawn (round bar (19-38 mm)) more
Yield Strength (Mpa) 415 
Elongation (%) 10 
Reduction in Area (%) 35 
Hardness (HB) 167  25  cold drawn (round bar (19-38 mm)) more