eFunda: Properties of Copper Alloy Copper Alloy UNS C65100
engineering fundamentals Copper Alloy Copper Alloy UNS C65100
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
UNS C65100
Conditions Tensile Properties 
T (°C)Treatment
25 (rod, wire, tube)  Tensile Strength (MPa) 276-655
Yield Strength (MPa) 103-476
Elongation (%) 55 
Reduction in Area (%)  
Note: Elongation is measured in 11 inches.
25 H80 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 450 
Yield Strength (MPa) 275 
Elongation (%) 20 
Reduction in Area (%)  
25 OS015 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 310 
Yield Strength (MPa) 140 
Elongation (%) 55 
Reduction in Area (%)  