eFunda: Properties of Copper Alloy Copper Alloy Copper Alloy UNS C65500
engineering fundamentals Copper Alloy Copper Alloy Copper Alloy UNS C65500
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
UNS C65500
Category Copper Alloy
Class Wrought
Type High-silicon bronze, A
Designations United States: UNS C65500

Composition
ElementWeight %
Cu  97.0 
Si  3.0 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 386-1000 25  (flat products, rod, wire, tube) more
Yield Strength (Mpa) 145-483
Elongation (%) 63 
Reduction in Area (%)  
Note: Elongation is measured in 3 inches.