eFunda: Properties of Copper Alloy UNS C95400
engineering fundamentals Copper Alloy UNS C95400
Directory | Career | News | Standards | Industrial | SpecSearch®
 
 
Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
UNS C95400
Category Copper Alloy
Class Cast
Type Aluminum bronze
Designations United States: UNS C95400, ASTM B148

Composition
ElementWeight %
Cu  85 
Fe  4 
Al  11 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 586 (724)  25  (castings: centrifugal, continuous, permanent mold, plaster, sand) 
Yield Strength (Mpa) 241 (372) 
Elongation (%) 18 (8) 
Reduction in Area (%)  
Note: Values in parentheses indicate responses to heat treatment
Hardness (HB) 170 (195)  25  (as cast) 
Note: Value in parentheses indicates response to heat treatment.