eFunda: Properties of Stainless Steel AISI Type 330
engineering fundamentals Stainless Steel AISI Type 330
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
AISI Type 330
Category Steel
Class Stainless steel
Type Austenitic standard
Common Names Chromium-Nickel steel
Designations  United States: AMS 5592 , AMS 5716 , ASTM B511 , ASTM B512 , ASTM B535 , ASTM B536 , ASTM B546 , SAE 30330 , SAE J405 (30330) , SAE J412 (30330) , UNS N08330

Composition

ElementWeight %
C  0.08 
Mn  2.00 
Si  0.75-1.5 
Cr  17.0-20.0 
Ni  34.0-37.0 
P  0.04 
S  0.03 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 196 25  
Tensile Strength (Mpa) 480  25  annealed (plate, sheet, strip) more
Yield Strength (Mpa) 210 
Elongation (%) 30 
Reduction in Area (%)  
Hardness (HRB) 75-85  25  annealed (plate, sheet, strip) 

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 14.4  0-100 more  
Thermal Conductivity (W/m-K) 12.5  24 more  
Specific Heat (J/kg-K) 460  0-100   

Electric Properties

Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 1020  25   