AISI Type 430F |
 |
|
| Category | Steel |
| Class | Stainless steel |
| Type | Ferritic standard |
| Common Names | Chromium steel |
| Designations |
France: AFNOR Z 10 CF 17 Germany: DIN 1.4104 Italy: UNI x 10 CrS 17 Japan: JIS SUS 430 Sweden: SS 2383 United States: ASTM A314 , ASTM A473 , ASTM A581 , ASTM A582 , MIL SPEC MIL-S-862 , SAE 51430F , SAE J405 (51430F) , UNS S43020
|
| Composition |
 |
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.8 |
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
200 |
25 |
|
| Tensile Strength (Mpa) |
722.5 |
25 |
annealed (wire) |
| Yield Strength (Mpa) |
105 |
| Elongation (%) |
|
| Reduction in Area (%) |
|
| Thermal Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Thermal Expansion (10-6/ºC) |
10.4 |
0-100 more |
|
| Thermal Conductivity (W/m-K) |
26.1 |
100 more |
|
| Specific Heat (J/kg-K) |
460 |
0-100 |
|
| Electric Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Electric Resistivity (10-9W-m) |
600 |
25 |
|
|