TM"> eFunda: Properties of Stainless Steel Stainless Steel Custom450<span class="footnotetext"><sup>TM</sup></span>
engineering fundamentals Stainless Steel Stainless Steel Custom450TM
Directory | Career | News | Industrial
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
TM">General Information
Further Details
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Custom450TM
ConditionsHardness
T (°C)TreatmentMethodValue
25 annealed (bar)  HRC 33 (max) 
25 annealed (plate, sheet, strip)  HRC 25 (min) 
25 H1000 (bar, plate, sheet, strip)  HRC 36 (min) 
25 H1150 (bar, plate, sheet, strip)  HRC 26 (min) 
25 H900 (bar, plate, sheet, strip)  HRC 40 (min) 