AISI A8 |
 |
|
| Category | Steel |
| Class | Tool steel |
| Type | Air-hardening medium-alloy cold work steel |
| Designations |
United States: ASTM A681 , FED QQ-T-570 , UNS T30108
|
| Composition |
 |
|
| Element | Weight % |
| C |
0.50-0.60 |
| Mn |
0.50 |
| Si |
0.75-1.10 |
| Cr |
4.75-5.50 |
| Ni |
0.30 |
| Mo |
1.15-1.65 |
| W |
1.00-1.50 |
| Cu |
0.25 |
| P |
0.03 |
| S |
0.03 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.87 |
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
| Thermal Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Thermal Expansion (10-6/ºC) |
12 |
20-425 more |
|
|