AISI P5 |
 |
|
| Category | Steel |
| Class | Tool steel |
| Type | Low-carbon mold steel |
| Designations |
United States: ASTM A681 , UNS T51605
|
| Composition |
 |
|
| Element | Weight % |
| C |
0.10 |
| Mn |
0.20-0.60 |
| Si |
0.40 |
| Cr |
2.00-2.50 |
| Ni |
0.35 |
| Cu |
0.25 |
| P |
0.03 |
| S |
0.03 |
|
|
| Mechanical Properties |
 |
|
| Properties | Conditions |
| T (°C) | Treatment |
| Density (×1000 kg/m3) |
7.8 |
25 |
|
| Poisson's Ratio |
0.27-0.30 |
25 |
|
| Elastic Modulus (GPa) |
190-210
|
25 |
|
|