Density
(Kg/m3)
Viscosity
(Pa-s)
Kinematic Viscosity
(m2/s)
Gas Constant
(J/kg·K)
Constant Pressure Spectfic Heat
(J/kg·K)
Constant Volume Specific Heat
(J/kg·K)
Specific Heat Ratio
0 1.29 1.71 × 10-5 1.33 × 10-5 287 1000 716 1.40
50 1.09 1.95 × 10-5 1.79 × 10-5 287 - - -
100 0.946 2.17 × 10-5 2.30 × 10-5 287 1010 723 1.40
150 0.835 2.38 × 10-5 2.85 × 10-5 287 - - -
200 0.746 2.57 × 10-5 3.45 × 10-5 287 1020 737 1.39
250 0.675 2.75 × 10-5 4.08 × 10-5 287 - - -
300 0.616 2.93 × 10-5 4.75 × 10-5 287 1040 758 1.38
400 0.525 3.25 × 10-5 6.20 × 10-5 287 1070 781 1.37
500 0.457 3.55 × 10-5 7.77 × 10-5 287 1090 805 1.36

 
Note: 1. All properties are under 1 atm (1.01325×105 Pa; 760 mmHg; 14.6959 psi) unless specified otherwise.