Heat Capacity: Silver
engineering fundamentals Heat Capacity: Silver
Directory | Career | News | Industrial
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Silver
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
298.15 100000 235
350 101325 236.9
400 101325 239.1
500 101325 244.4
600 101325 250.2
Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise