Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 790.5
250 101325 855.4
298.15 100000 897
350 101325 930.6
400 101325 955.5
500 101325 994.8
600 101325 1034