Calcium
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 612.3
250 101325 634
298.15 100000 647
350 101325 656.7
400 101325 670.4
500 101325 710.9
600 101325 758