Heat Capacity: Cobalt
engineering fundamentals Heat Capacity: Cobalt
Directory | Career | News | Industrial
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Cobalt
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 377.2
250 101325 406.9
298.15 100000 421
350 101325 435.7
400 101325 450.2
500 101325 478.5
600 101325 503.3