Chromium
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 382
250 101325 428.9
298.15 100000 449
350 101325 469.1
400 101325 485.2
500 101325 512.2
600 101325 533.1