Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 356.1
250 101325 374.1
298.15 100000 385
350 101325 392.6
400 101325 398.6
500 101325 407.7
600 101325 416.7