Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 386.6
250 101325 425.1
298.15 100000 449
350 101325 470.6
400 101325 490.5
500 101325 531.8
600 101325 573.9