Magnesium
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 934.8
250 101325 988.3
298.15 100000 1023
350 101325 1052
400 101325 1075
500 101325 1118
600 101325 1159