Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 419.6
250 101325 454.1
298.15 100000 479
350 101325 500.9
400 101325 519.3
500 101325 551.3
600 101325 580.7