Lead
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 124.9
250 101325 127.2
298.15 100000 129
350 101325 131.8
400 101325 133.8
500 101325 137.8
600 101325 141.9