Heat Capacity: Silicon
engineering fundamentals Heat Capacity: Silicon
Directory | Career | News | Industrial
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Silicon
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 556.9
250 101325 648.7
298.15 100000 705
350 101325 757.7
400 101325 788.3
500 101325 830.7
600 101325 859.9