Heat Capacity: Tantalum
engineering fundamentals Heat Capacity: Tantalum
Directory | Career | News | Industrial
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Tantalum
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 133.1
250 101325 137.4
298.15 100000 140
350 101325 141.5
400 101325 142.8
500 101325 145.6
600 101325 148.3