Heat Capacity: Titanium
engineering fundamentals Heat Capacity: Titanium
Directory | Career | News | Standards | Industrial | SpecSearch®
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Titanium
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 467.3
250 101325 502.9
298.15 100000 523
350 101325 546.7
400 101325 561.1
500 101325 582.4
600 101325 597.5