Tungsten
 
Conditions Heat Capacity (J/Kg-K)
Temperature (K) Pressure (Pa)
200 101325 122.3
250 101325 128.9
298.15 100000 132
350 101325 134.1
400 101325 135.6
500 101325 137.9
600 101325 140.3