Aluminum
 
Conditions Thermal Conductivity (W/m-K)
Temperature (K) Pressure (Pa)
1 101325 4110
2 101325 8180
3 101325 12100
4 101325 15700
5 101325 18800
6 101325 21300
7 101325 22900
8 101325 23700
9 101325 23900
10 101325 23500
15 101325 17600
20 101325 11700
30 101325 4950
40 101325 2400
50 101325 1350
60 101325 850
70 101325 585
80 101325 432
90 101325 342
100 101325 302
150 101325 248
200 101325 237
250 101325 235
300 101325 237
350 101325 240
400 101325 240
500 101325 236
600 101325 231
800 101325 218