Thermal Conductivity: Copper
engineering fundamentals Thermal Conductivity: Copper
Directory | Career | News | Standards | Industrial | SpecSearch®
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Copper
 
Conditions Thermal Conductivity (W/m-K)
Temperature (K) Pressure (Pa)
1 101325 4220
2 101325 8400
3 101325 12500
4 101325 16200
5 101325 19500
6 101325 22200
7 101325 23900
8 101325 24800
9 101325 24900
10 101325 24300
15 101325 17100
20 101325 10800
30 101325 4450
40 101325 2170
50 101325 1250
60 101325 829
70 101325 647
80 101325 557
90 101325 508
100 101325 482
150 101325 429
200 101325 413
250 101325 406
300 101325 401
350 101325 396
400 101325 393
500 101325 386
600 101325 379
800 101325 366
1000 101325 352
1200 101325 339