Thermal Conductivity: Magnesium
engineering fundamentals Thermal Conductivity: Magnesium
Directory | Career | News | Standards | Industrial | SpecSearch®
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Magnesium
 
Conditions Thermal Conductivity (W/m-K)
Temperature (K) Pressure (Pa)
1 101325 986
2 101325 1960
3 101325 2900
4 101325 3760
5 101325 4500
6 101325 5080
7 101325 5470
8 101325 5670
9 101325 5700
10 101325 5580
15 101325 4110
20 101325 2720
30 101325 1290
40 101325 719
50 101325 465
60 101325 327
70 101325 249
80 101325 202
90 101325 178
100 101325 169
150 101325 161
200 101325 159
250 101325 157
300 101325 156
350 101325 155
400 101325 153
500 101325 151
600 101325 149
800 101325 146