Conditions Thermal Conductivity (W/m-K)
Temperature (K) Pressure (Pa)
1 101325 1.44
2 101325 2.88
3 101325 4.32
4 101325 5.75
5 101325 7.19
6 101325 8.63
7 101325 10.1
8 101325 11.5
9 101325 12.9
10 101325 14.3
15 101325 21.2
20 101325 27.5
30 101325 36.5
40 101325 39
50 101325 37.4
60 101325 35.5
70 101325 34
80 101325 32.6
90 101325 31.5
100 101325 30.5
150 101325 27
200 101325 24.5
250 101325 22.9
300 101325 21.9
350 101325 21
400 101325 20.4
500 101325 19.7
600 101325 19.4
800 101325 19.7
1000 101325 20.7
1200 101325 22
1400 101325 23.6
1600 101325 25.3
1800 101325 27