Thermal Conductivity: Tungsten
engineering fundamentals Thermal Conductivity: Tungsten
Directory | Career | News | Industrial
Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Tungsten
 
Conditions Thermal Conductivity (W/m-K)
Temperature (K) Pressure (Pa)
1 101325 1440
2 101325 2870
3 101325 4280
4 101325 5630
5 101325 6870
6 101325 7950
7 101325 8800
8 101325 9380
9 101325 9680
10 101325 9710
15 101325 7200
20 101325 4050
30 101325 1440
40 101325 692
50 101325 427
60 101325 314
70 101325 258
80 101325 229
90 101325 217
100 101325 208
150 101325 192
200 101325 185
250 101325 180
300 101325 174
350 101325 167
400 101325 159
500 101325 146
600 101325 137
800 101325 125
1000 101325 118
1200 101325 112
1400 101325 108
1600 101325 104
1800 101325 101
2000 101325 98