eFunda Polymers: Listing of Polyphthalamide
engineering fundamentals Polyphthalamide
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
Introduction

Polyphthalamide, also known as PTA,.
  - It is a thermoplastic polycondensate.

Top of Page

Specific Grades of Polyphthalamide
1. Polyphthalamide, extra tough.
2. Polyphthalamide, 45% glass reinforced.
3. Polyphthalamide, 33% glass reinforced, V-0.
4. Polyphthalamide, 40% mineral reinforced.
5. Polyphthalamide, 40% glass / mineral reinforced, heat stablized.
6. Polyphthalamide, 50% glass / mineral reinforced, V-0.
7. Polyphthalamide, 51% glass / mineral reinforced.
8. Polyphthalamide, 15% glass reinforced.
9. Polyphthalamide, 15% glass reinforced, V-0.
10. Polyphthalamide, 45% glass reinforced, V-0.
11. Polyphthalamide, 40% glass / mineral reinforced.
12. Polyphthalamide, 40% mineral reinforced, heat stablized.

Top of Page