eFunda Polymers: Properties of ABS {40% long glass fiber reinforced, injection molding grade}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...)
Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
Thermoplastic/Thermoset
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography
Login

Home Membership Magazines Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
ABS
 
List of Suppliers
Additives: 40% long glass fiber reinforced
Application: injection molding grade
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)   6900  tensile   D638
Flexural Modulus (MPa)   7590   23 ºC   D790
Tensile Strength (MPa)  110 at break   D638
Compressive Strength (MPa)
at yield or break
 117     D695
Flexural Strength (MPa)
at yield or break
 173     D790
Elongation at break (%)   2     D638
Hardness   90 - 100  Rockwell M   D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  1.3     D256A

 Thermal Properties Conditions
Pressure State ASTM
Deflection Temperature (ºC)  107   0.46 MPa   D648
 102   1.82 MPa   D648

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.36   D792
Water Absorption (% weight increase)  0.2  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)  100 - 110  Tg, amorphous  
Processing Temperature (ºC)  204 - 238  injection molding  
Linear Mold Shrinkage (cm/cm)  0.001   D955