eFunda Polymers: Properties of Polyethylene and ethylene copolymers {ethylene / methyl acrylate, low density copolymer}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Polyethylene and ethylene copolymers
 
List of Suppliers
State: ethylene / methyl acrylate, low density copolymer
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)   83  tensile   D638
Tensile Strength (MPa)   12 at break   D638
  12 at yield   D638
Elongation at break (%)   740     D638

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  0.942 - 0.945   D792
Water Absorption (% weight increase)  0  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)   83  Tm, crystalline  
Processing Temperature (ºC)   94 - 327  extrusion  

Top of Page

Suppliers
A. Schulman Akron, OH  800-662-7203
Chevron Chemical Co. Houston, TX  800-231-3828
Exxon Chemical Co. Houston, TX  800-231-6633
Network Polymers, Inc. Akron, OH  888-437-4674

Top of Page

Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise

Copyright © 2009 eFunda, Inc.