25% Off
Exclusive partnership offers for efunda users.
|
|
Polyethylene and ethylene copolymers |
|
| State: |
high density homopolymer |
|
| Material Properties |
 |
|
| Mechanical Properties |
Conditions |
| Thermal Properties |
Conditions |
| Physical & Electrical Properties |
Conditions |
| Processing Properties |
Conditions |
|
|
|
| Suppliers |
 |
|
|
A. Schulman |
Akron, OH |
800-662-7203 |
|
American Polymers, Inc. |
Worcester, MA |
|
|
Bamberger Polymers, Inc. |
Jericho, NY |
|
|
Chevron Chemical Co. |
Houston, TX |
800-231-3828 |
|
Dow Plastics |
Midland, MI |
800-441-4369 |
|
Eastman Chemical Co. |
Kingsport, TN |
800-327-8626 |
|
Equistar Chemicals LP |
Houston, TX |
888-777-0232 |
|
Exxon Chemical Canada |
Toronto, Ontario, M5W 1K3, Canada |
|
|
Exxon Chemical Co. |
Houston, TX |
800-231-6633 |
|
Federal Plastics Corp. |
Cranford, NJ |
800-541-4424 |
|
Fina Oil & Chemical Co. |
Dallas, TX |
800-344-3462 |
|
M.A. Industries, Inc. |
Peachtree City, GA |
800-241-8250 |
|
Mobil Chemical Co. |
Edison, NJ |
|
|
Network Polymers, Inc. |
Akron, OH |
888-437-4674 |
|
NOVA Chemicals, Ltd. |
Calgary, Alberta T2P 5C6, Canada |
|
|
Phillips Chemical Co. |
Bartlesville, OK |
800-537-3746 |
|
R.S.G. Polymers Corp. |
Stony Brook, NY |
|
|
Shuman Plastics, Inc. |
Depew, NY |
|
|
Solvay Polymers, Inc. |
Houston, TX |
800-231-6313 |
|
Ticona |
Summit, NJ |
800-526-4960 |
|
Union Carbide Corp. |
Danbury, CT |
800-335-8550 |
|
|