eFunda Polymers: Properties of Polystyrene and styrene copolymers {copolymer, impact modified, high heat resistant}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Polystyrene and styrene copolymers
 
List of Suppliers
State: copolymer
Additives: impact modified
Application: high heat resistant
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)   1932 - 2277  tensile   D638
Flexural Modulus (MPa)   2208 - 2553   23 ºC   D790
Tensile Strength (MPa)   32 - 41 at break   D638
Flexural Strength (MPa)
at yield or break
  59 - 73     D790
Elongation at break (%)   10 - 20     D638
Hardness   75 - 95  Rockwell R   D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  0.8 - 2.1     D256A

 Thermal Properties Conditions
Pressure State ASTM
Coef of Thermal Expansion (10-6/ºC)   67 - 79     D696
Deflection Temperature (ºC)  110 - 127   1.82 MPa   D648

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.05 - 1.08   D792
Water Absorption (% weight increase)  0.1  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Melt Flow (gm/10 min)  1 - 1.8   D1238
Processing Temperature (ºC)  219 - 283  injection molding  
 205 - 260  extrusion  
Linear Mold Shrinkage (cm/cm)  0.003 - 0.006   D955

Top of Page

Suppliers
Bayer Corp. Pittsburgh, PA  800-662-2927
NOVA Chemicals, Ltd. Calgary, Alberta T2P 5C6, Canada   

Top of Page

Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise

Copyright © 2009 eFunda, Inc.