eFunda Polymers: Properties of Ketones {poly(etherether-ketone), 30% carbon fiber reinforced}
engineering fundamentals Polymer Material Properties
Directory | Career | News | Standards | Industrial | SpecSearch®
Generic (ABS, ...) Trade Name
Materials Home
General Information
Polymer Home
Glossary
Material Science
Overview
Characteristics
Comparisons
Selection Criteria
Applications
Flow Characteristics
Datasheet Primer
Major Categories
Polymer Index
History Timeline
List by Process
List by ThermoP/S
Specific Polymer
Category / Grades
Datasheet
Supplier Info
Resources
Bibliography


Login

Home Membership Store Forum Search Member Calculators

Materials

Design

Processes

Units

Formulas

Math
 
Ketones
 
List of Suppliers
State: poly(etherether-ketone)
Additives: 30% carbon fiber reinforced
Material Properties
 Mechanical Properties Conditions
State 1 State 2 ASTM
Elastic Modulus (MPa)  12972 - 24150  tensile   D638
Flexural Modulus (MPa)  12834 - 17940   23 ºC   D790
 12558   94 ºC   D790
 12075  122 ºC   D790
  9660  149 ºC   D790
Tensile Strength (MPa)  206 - 228 at break   D638
Compressive Strength (MPa)
at yield or break
 173 - 238     D695
Flexural Strength (MPa)
at yield or break
 276 - 332     D790
Elongation at break (%)   1 - 4     D638
Izod Impact (J/cm of notch)
1/8" thick specimen unless noted
  0.8 - 1.1     D256A

 Thermal Properties Conditions
Pressure State ASTM
Coef of Thermal Expansion (10-6/ºC)   5 - 44    > 150 ºC D696
Coef of Thermal Expansion (10-6/ºC)   15 - 22    < 150 ºC D696
Deflection Temperature (ºC)  324   0.46 MPa   D648
 288 - 322   1.82 MPa   D648
Thermal Conductivity (W/m-ºC)  0.205     C177

 Physical & Electrical Properties Conditions
State ASTM
Specific Gravity  1.42 - 1.44   D792
Water Absorption (% weight increase)  0.06  saturated D570
 0.06 - 0.12  after 24 hrs D570

 Processing Properties Conditions
Type ASTM
Melting Temperature (ºC)  334  Tm, crystalline  
Processing Temperature (ºC)  349 - 427  injection molding  
Molding Pressure (MPa)   69 - 138    
Compression Ratio  2    
Linear Mold Shrinkage (cm/cm)  0.0005 - 0.014   D955

Top of Page

Suppliers
DSM Engineering Plastic Products, Inc. Reading, PA  800-729-0101
LNP Engineering Plastics, Inc. Exton, PA  800-854-8774
RTP Co. Winona, MN  800-433-4787
Victrex USA West Chester, PA  800-842-8739

Top of Page

Home  Membership  About Us  Privacy  Disclaimer  Contact  Advertise

Copyright © 2009 eFunda, Inc.