Steel Wide Flange I-Beams
Directory
|
Career
|
News
|
Standards
|
Industrial
|
SpecSearch®
Geometry Home
Cross-Sections of
Standard Beams
Steel S-Type I-beam
Steel W-Type I-beam
Steel Channels
Steel Angles
Aluminum I-Beams
Aluminum Channels
Common Beams
Applications
Beam Bending
Geometric Shapes
Common Areas
Common Solids
Useful Geometry
Resources
Bibliography
Login
Home
Membership
Magazines
Forum
Search Member
Calculators
Materials
Design
Processes
Units
Formulas
Math
Browse all »
Technology Guide »
Demonstrations »
MathWorld
™ »
Industry Solutions »
Steel Wide Flange I-Beams
The I-Beams are identified by:
W DEPTH (inches) × WEIGHT PER UNIT LENGTH (pound force per foot)
For Example:
W27 × 161
is an I-Beam with a Depth of 27 inches and having a Nominal Weight per Foot of 161 lbf/ft.
Check all the I-beams you would like to see properties for and then click GET.
ALL
W27 × ___
W24 × ___
W21 × ___
W18 × ___
W16 × ___
W27 × 178
W24 × 162
W21 × 147
W18 × 119
W16 × 100
W27 × 161
W24 × 146
W21 × 132
W18 × 106
W16 × 89
W27 × 146
W24 × 131
W21 × 122
W18 × 97
W16 × 77
W27 × 114
W24 × 117
W21 × 111
W18 × 86
W16 × 67
W27 × 102
W24 × 104
W21 × 101
W18 × 76
W16 × 57
W27 × 94
W24 × 94
W21 × 93
W18 × 71
W16 × 50
W27 × 84
W24 × 84
W21 × 83
W18 × 65
W16 × 45
W24 × 76
W21 × 73
W18 × 60
W16 × 40
W24 × 68
W21 × 68
W18 × 55
W16 × 36
W24 × 62
W21 × 62
W18 × 50
W16 × 31
W24 × 55
W21 × 57
W18 × 46
W16 × 26
W21 × 50
W18 × 40
W21 × 44
W18 × 35
W14 × ___
W12 × ___
W10 × ___
W8 × ___
W6 × ___
W14 × 665
W12 × 336
W10 × 112
W8 × 67
W6 × 20
W14 × 605
W12 × 305
W10 × 100
W8 × 58
W6 × 16
W14 × 550
W12 × 279
W10 × 88
W8 × 48
W6 × 15
W14 × 500
W12 × 252
W10 × 77
W8 × 40
W6 × 12
W14 × 455
W12 × 230
W10 × 68
W8 × 35
W6 × 9
W14 × 426
W12 × 210
W10 × 60
W8 × 31
W14 × 398
W12 × 190
W10 × 54
W8 × 28
W5 × ___
W14 × 370
W12 × 170
W10 × 49
W8 × 24
W5 × 19
W14 × 342
W12 × 152
W10 × 45
W8 × 21
W5 × 16
W14 × 311
W12 × 136
W10 × 39
W8 × 18
W14 × 283
W12 × 120
W10 × 33
W8 × 15
W4 × ___
W14 × 257
W12 × 106
W10 × 30
W8 × 13
W4 × 13
W14 × 233
W12 × 96
W10 × 26
W8 × 10
W14 × 211
W12 × 87
W10 × 22
W14 × 193
W12 × 79
W10 × 19
W14 × 176
W12 × 72
W10 × 17
W14 × 159
W12 × 65
W10 × 15
W14 × 145
W12 × 58
W10 × 12
W14 × I32
W12 × 53
W14 × 120
W12 × 50
W14 × 109
W12 × 45
W14 × 99
W12 × 40
W14 × 90
W12 × 35
W14 × 82
W12 × 30
W14 × 74
W12 × 26
W14 × 68
W12 × 22
W14 × 61
W12 × 19
W14 × 53
W12 × 16
W14 × 48
W12 × 14
W14 × 43
W14 × 38
W14 × 34
W14 × 30
W14 × 26
W14 × 22
ALL