slug per cubic foot 
Symbol:  slug/ft3 
Category:  Density 
SI Equivalent:  515.379 kg/m3
Dimension ML-3 
System:  UK, US 
 Download a Palm version of this unit conversion calculator!
Convert     slug/ft3  
1 slug/ft3 = 
Density
  Symbol Unit Name
0.515379  g/cm3  gram per cubic centimeter 
5.15379×105  g/m3  gram per cubic meter 
515.379  g/l  gram per liter 
0.515379  kg/dm3  kilogram per cubic decimeter 
515.379  kg/m3  kilogram per cubic meter 
0.515379  kg/l  kilogram per liter 
514.785  oz (av.)/ft3  ounce (av.) per cubic foot 
0.297908  oz (av.)/in3  ounce (av.) per cubic inch 
32.174  lbm/ft3  pound mass per cubic foot 
1.86192×10-2  lbm/in3  pound mass per cubic inch 
868.699  lbm/yd3  pound mass per cubic yard 
5.16534  lbm/gal (UK)  pound mass per gallon (UK) 
4.30104  lbm/gal (US, liq.)  pound mass per gallon (US, liq.) 
5.78704×10-4  slug/in3  slug per cubic inch 
27  slug/yd3  slug per cubic yard 
0.515379    specific gravity 