Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
AISI 1340
ConditionsImpact Energy (J)
T (°C)TreatmentMethodValue
25 annealed at 800°C   Izod 70.5 
25 normalized at 870°C   Izod 92.5 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.