Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
AISI 4340
ConditionsHardness
T (°C)TreatmentMethodValue
25 annealed at 810°C   HB 217 
25 normalized at 870°C   HB 363 
25 oil quenched, fine grained, tempered at 205°C   HB 520 
25 oil quenched, fine grained, tempered at 315°C   HB 486 
25 oil quenched, fine grained, tempered at 425°C   HB 430 
25 oil quenched, fine grained, tempered at 540°C   HB 360 
25 oil quenched, fine grained, tempered at 650°C   HB 280 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.