| SAE 945A | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | (sheet and strip, plate, shapes and bar to 13 mm) | Tensile Strength (MPa) | 450 |
| Yield Strength (MPa) | 310 | ||
| Elongation (%) | 22 | ||
| Reduction in Area (%) | |||
| 25 | (sheet and strip) | Tensile Strength (MPa) | 415 |
| Yield Strength (MPa) | 310 | ||
| Elongation (%) | 22 | ||
| Reduction in Area (%) | |||
| 25 | (sheet and strip, plate, shapes and bar to 13-38 mm) | Tensile Strength (MPa) | 425 |
| Yield Strength (MPa) | 290 | ||
| Elongation (%) | 24 | ||
| Reduction in Area (%) | |||
| 25 | (sheet and strip, plate, shapes and bar to 38-76 mm) | Tensile Strength (MPa) | 425 |
| Yield Strength (MPa) | 276 | ||
| Elongation (%) | 24 | ||
| Reduction in Area (%) | |||