Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
SAE 945C
Conditions Tensile Properties 
T (°C)Treatment
25 (sheet and strip)  Tensile Strength (MPa) 415 
Yield Strength (MPa) 310 
Elongation (%) 22 
Reduction in Area (%)  
25 (sheet and strip, plate, shapes and bar to 38-76 mm)  Tensile Strength (MPa) 425 
Yield Strength (MPa) 276 
Elongation (%) 24 
Reduction in Area (%)  
25 (sheet and strip, plate, shapes and bar to 13-38 mm)  Tensile Strength (MPa) 425 
Yield Strength (MPa) 290 
Elongation (%) 24 
Reduction in Area (%)  
25 (sheet and strip, plate, shapes and bar to 13 mm)  Tensile Strength (MPa) 450 
Yield Strength (MPa) 310 
Elongation (%) 22 
Reduction in Area (%)  
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.