Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Further Details
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
SAE 950D
Conditions Tensile Properties 
T (°C)Treatment
25 (sheet and strip, plate, shapes and bar to 38-76 mm)  Tensile Strength (MPa) 460 
Yield Strength (MPa) 310 
Elongation (%) 24 
Reduction in Area (%)  
25 (sheet and strip, plate, shapes and bar to 13-38 mm)  Tensile Strength (MPa) 485 
Yield Strength (MPa) 345 
Elongation (%) 22 
Reduction in Area (%)  
25 (sheet and strip, plate, shapes and bar to 13 mm)  Tensile Strength (MPa) 485 
Yield Strength (MPa) 345 
Elongation (%) 22 
Reduction in Area (%)  
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.