Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Laser Focus World

Semiconductors, medical equipment, lasers, optics and aviation and aerospace.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Offshore

International news and technology for marine/offshore operations around the world.

more free magazines
 
AISI Type 305
Category Steel
Class Stainless steel
Type Austenitic standard
Common Names Chromium-Nickel steel
Designations  Germany: DIN 1.4303
Italy: UNI X 8 CrNi 19 10
Japan: JIS SUS 305 , JIS SUS 305 J1
United States: AMS 5514 , AMS 5685 , AMS 5686 , ASME SA193 , ASME SA194 , ASME SA240 , ASTM A167 , ASTM A240 , ASTM A249 , ASTM A276 , ASTM A313 , ASTM A314 , ASTM A368 , ASTM A473 , ASTM A478 , ASTM A492 , ASTM A493 , ASTM A511 , ASTM A554 , ASTM A580 , FED QQ-S-763 , FED QQ-W-423 , SAE 30305 , SAE J405 (30305) , UNS S30500

Composition

ElementWeight %
C  0.12 
Mn  2.00 
Si  1.00 
Cr  17.0-19.0 
Ni  10.5-13.0 
P  0.045 
S  0.03 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 193 25  
Tensile Strength (Mpa) 515  25  hot finished and annealed (plate, sheet, strip) more
Yield Strength (Mpa) 205 
Elongation (%) 40 
Reduction in Area (%) 50 
Hardness (HRB) 88 (max)  25  annealed (plate, sheet, strip) 

Thermal Properties

Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 17.2  0-100 more  
Thermal Conductivity (W/m-K) 16.2  100 more  
Specific Heat (J/kg-K) 500  0-100   

Electric Properties

Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 720  25   