Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

World Pumps

Major news, innovation and real-life applications for pumps and ancillary equipment.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

more free magazines
 
E-Brite26-1
Category Steel
Class Stainless steel
Type Ferritic nonstandard

Composition

ElementWeight %
C  0.01 
Mn  0.40 
Si  0.40 
Cr  25.0-27.5 
Ni  0.5 
P  0.02 
S  0.02 
Mo  0.75-1.5 
N  0.015 
Cu  0.2 
Ni+Cu  0.5 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 450  25  annealed, hot finished (plate, sheet, strip) more
Yield Strength (Mpa) 275 
Elongation (%) 20 
Reduction in Area (%) 45 
Hardness (HRB) 90 (max)  25  annealed (plate, sheet, strip) 