Metal Alloys
Alloy Home
Steels
Alloy Steels
General Information
Properties
Classification
Standard
H-Steels
HSLA
Alloy Steel List
AISI 1xxx
AISI 2xxx
AISI 3xxx
AISI 4xxx
AISI 5xxx
AISI 6xxx
AISI 8xxx
AISI 9xxx
* For other AISI or Non-AISI, please use the search function above or check Grades.
ASTM Steels
Specific Alloy Steel
General Information
Resources
Bibliography
Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Reinforced Plastics

Informed and impartial coverage on the global composites industry.

Offshore

International news and technology for marine/offshore operations around the world.

more free magazines
 
Nitronic32
Category Steel
Class Stainless steel
Type Austenitic nonstandard

Composition

ElementWeight %
C  0.10 
Mn  12.00 
Si  0.50 
Cr  18.0 
Ni  1.6 
N  0.35 

Mechanical Properties

Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 690  25  annealed (wire) more
Yield Strength (Mpa) 380 
Elongation (%) 30 
Reduction in Area (%) 50 
Glossary