Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
 1-30 (of 43 found)  next >>
Aluminum Alloy
Name Type
201.0  Cast 
206.0  Cast 
208.0  Cast 
242.0  Cast 
295.0  Cast 
296.0  Cast 
308.0  Cast 
319.0  Cast 
336.0  Cast 
354.0  Cast 
355.0  Cast 
356.0  Cast 
357.0  Cast 
359.0  Cast 
360.0  Cast 
380.0  Cast 
383.0  Cast 
384.0  Cast 
390.0  Cast 
413.0  Cast 
443.0  Cast 
514.0  Cast 
518.0  Cast 
520.0  Cast 
535.0  Cast 
712.0  Cast 
713.0  Cast 
771.0  Cast 
850.0  Cast 
A206.0  Cast 
 1-30 (of 43 found)  next >>
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.