Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Wind Systems

Towers, turbines, gearboxes; processes for shaping and finishing component parts.

more free magazines
 
AA 1350
ConditionsShear Strength (MPa)
T (°C)Treatment
25 H12   62 
25 H14   69 
25 H16   76 
25 H19   105 
25 O   55 