Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Further Details
Resources
Bibliography
Chemical Engineering

The industry gateway for chemical engineering and plant operations.

Reinforced Plastics

Informed and impartial coverage on the global composites industry.

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free magazines
 
AA 1350
Conditions Tensile Properties 
T (°C)Treatment
25 H12   Tensile Strength (MPa) 97 
Yield Strength (MPa) 83 
Elongation (%)  
Reduction in Area (%)  
25 H14   Tensile Strength (MPa) 110 
Yield Strength (MPa) 97 
Elongation (%)  
Reduction in Area (%)  
25 H16   Tensile Strength (MPa) 125 
Yield Strength (MPa) 110 
Elongation (%)  
Reduction in Area (%)  
25 H19   Tensile Strength (MPa) 185 
Yield Strength (MPa) 165 
Elongation (%) 1.5 
Reduction in Area (%)  
25 O   Tensile Strength (MPa) 83 
Yield Strength (MPa) 28 
Elongation (%) 23 
Reduction in Area (%)  