| 319.0 | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | F (permanent mold casting) | Tensile Strength (MPa) | 235 |
| Yield Strength (MPa) | 130 | ||
| Elongation (%) | 2.5 | ||
| Reduction in Area (%) | |||
| 25 | F (sand casting) | Tensile Strength (MPa) | 185 |
| Yield Strength (MPa) | 125 | ||
| Elongation (%) | 2.0 | ||
| Reduction in Area (%) | |||
| 25 | T6 (permanent mold casting) | Tensile Strength (MPa) | 280 |
| Yield Strength (MPa) | 185 | ||
| Elongation (%) | 3.0 | ||
| Reduction in Area (%) | |||
| 25 | T6 (sand casting) | Tensile Strength (MPa) | 250 |
| Yield Strength (MPa) | 165 | ||
| Elongation (%) | 2.0 | ||
| Reduction in Area (%) | |||